Chemical Component

High molecular polymer containing conductive carbon structure material affinity group

Tech Data

Appearance: light yellow viscous liquid to paste

Active ingredient: 100%

pH value (1% aqueous solution): 8.0-9.0

Property

  1. Prevent powder flocculation, increase system storage stability, and achieve low resistivity.
  2. Improve grinding efficiency, reduce viscosity, and increase slurry solid content.
  3. Suitable for dispersion of graphene, conductive carbon black, carbon nanotubes, graphite, etc.

Application

Dispersion of nanopowders such as graphene, conductive carbon black, carbon nanotubes, graphite, etc. in water and NMP.

Dispersion of nanopowders such as graphene, conductive carbon black, carbon nanotubes, graphite, etc. in water and NMP.

Dosage Advice

Powder type                                  Dosage

(SF-D495/Powder %)

Graphene                                      40-80

Carbon Nanotubes                       40-80

Conductive carbon black              20-80          

Method

It is recommended to completely dissolve the dispersant in the grinding medium first and then add the powder for grinding.

Package

Net weight:50kg/drum

Store in a cool, dry place in a sealed container for 2 years.